FEATURESHigh quality abrasion resistant rubberExcellent wear resistanceHigh hardness aluminium oxide tilesvickers harxFFFDdness 1000Excellent wear resistanceTiles cushioned from impactReliable resu ID: 454302

FEATURESHigh quality abrasion resistant rubberExcellent

Share:

Link:

Embed:

Download Presentation from below link

Download Pdf The PPT/PDF document "HOT VULCANISED CERAMIC LAGGING" is the property of its rightful owner. Permission is granted to download and print the materials on this web site for personal, non-commercial use only, and to display it on your personal computer provided you do not modify the materials and that you retain all copyright notices contained in the materials. By downloading content from our website, you accept the terms of this agreement.


Presentation Transcript

HOT VULCANISED CERAMIC LAGGING FEATURESHigh quality abrasion resistant rubberExcellent wear resistanceHigh hardness aluminium oxide tilesvickers har�dness 1000Excellent wear resistanceTiles cushioned from impactReliable resultElastotec approved applicatorsReliable resultFeatures & BenetsElastotec has pioneered the development of Hot Vulcanised (HV) Ceramic Lagging and the method for applying this to the pulley. This process has been patented and a network of “Approved Applicators” has been established to provide end users with the best Ceramic Lagging that has been applied to Elastotec OEM specications. The HV Ceramic Lagging has no joins and as a result does not suffer from pulley shell corrosion that leads to lagging failure.Additionally the HV bonding process provides consistent 100% rubber tear bonds ensuring the longest possible service life for the pulley.HV Ceramic Lagging represents a signicant advancement in technology and should be considered by all bulk materials handling sites that are looking for increased reliability and reduced down time. www.elastotec.com.au COLD VULCANISING Minimal Rubber Tear100% Rubber TearAdhesion strengthStable rubber hardnessRoom temperatureBonding pressureBonding pressure durationBond failure JOINS EVERY 250MMNO BODING LAYER ON SIDES OF THE LAGGINGBODING LAYER ON SIDES OF THE LAGGINGBUFFED BONDING LAYERUNCURED BONDING LAYER NO JOINTSHOT VULCANISEDCERAMIC LAGGING JOINS EVERY 250MMNO BODING LAYER ON SIDES OF THE LAGGINGBODING LAYER ON SIDES OF THE LAGGINGBUFFED BONDING LAYERUNCURED BONDING LAYER NO JOINTSHOT VULCANISEDCERAMIC LAGGING JOINS EVERY 250MMNO BODING LAYER ON SIDES OF THE LAGGINGBODING LAYER ON SIDES OF THE LAGGINGBUFFED BONDING LAYERUNCURED BONDING LAYER NO JOINTSHOT VULCANISEDCERAMIC LAGGING Buffed bonding layer JOINS EVERY 250MMNO BODING LAYER ON SIDES OF THE LAGGINGBODING LAYER ON SIDES OF THE LAGGINGBUFFED BONDING LAYERUNCURED BONDING LAYER NO JOINTSHOT VULCANISEDCERAMIC LAGGING JOINS EVERY 250MMNO BODING LAYER ON SIDES OF THE LAGGINGBODING LAYER ON SIDES OF THE LAGGINGBUFFED BONDING LAYERUNCURED BONDING LAYER NO JOINTSHOT VULCANISEDCERAMIC LAGGING Uncured bonding layer JOINS EVERY 250MMNO BODING LAYER ON SIDES OF THE LAGGINGBODING LAYER ON SIDES OF THE LAGGINGBUFFED BONDING LAYERUNCURED BONDING LAYER NO JOINTSHOT VULCANISEDCERAMIC LAGGING www.elastotec.com.au