Damaged area ground out ready to be furnace brazed. Damaged area ground out ready to be furnace brazed.

Damaged area ground out ready to be furnace brazed. - PowerPoint Presentation

stefany-barnette
stefany-barnette . @stefany-barnette
Follow
392 views
Uploaded On 2016-09-12

Damaged area ground out ready to be furnace brazed. - PPT Presentation

Furnace brazing requires 1000 degrees pre heat and then a slow cool down period Furnace brazing completed and slow cooling Ready to hand finish Hand finished and ready to be painted ID: 465157

furnace ready slow hand ready furnace hand slow brazing

Share:

Link:

Embed:

Download Presentation from below link

Download Presentation The PPT/PDF document "Damaged area ground out ready to be furn..." is the property of its rightful owner. Permission is granted to download and print the materials on this web site for personal, non-commercial use only, and to display it on your personal computer provided you do not modify the materials and that you retain all copyright notices contained in the materials. By downloading content from our website, you accept the terms of this agreement.


Presentation Transcript

Slide1
Slide2

Damaged area ground out ready to be furnace brazed.Slide3

Furnace brazing requires 1,000 degrees pre heat and then a slow cool down period.Slide4

Furnace brazing completed and slow cooling.Slide5

Ready to hand finishSlide6